Load-Bearing and Machining Behavior of Treated Nano-sorghum-Millet-Husk-Biosilica- and Kenaf-Fiber-Reinforced Vinyl Ester Composite
Vol. 25, No. 11, pp. 4387-4399, Nov. 2024

Abstract
Statistics
Cumulative Counts from November, 2022
Multiple requests among the same browser session are counted as one view. If you mouse over a chart, the values of data points will be shown.
Multiple requests among the same browser session are counted as one view. If you mouse over a chart, the values of data points will be shown.
|
Cite this article
[IEEE Style]
G. Ananth, G. Ananth, S. Thirugnanam, S. Rajaram, "Load-Bearing and Machining Behavior of Treated Nano-sorghum-Millet-Husk-Biosilica- and Kenaf-Fiber-Reinforced Vinyl Ester Composite," Fibers and Polymers, vol. 25, no. 11, pp. 4387-4399, 2024. DOI: 10.1007/s12221-024-00736-9.
[ACM Style]
G Ananth, G Ananth, S Thirugnanam, and Srinivasan Rajaram. 2024. Load-Bearing and Machining Behavior of Treated Nano-sorghum-Millet-Husk-Biosilica- and Kenaf-Fiber-Reinforced Vinyl Ester Composite. Fibers and Polymers, 25, 11, (2024), 4387-4399. DOI: 10.1007/s12221-024-00736-9.